Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 216 °C @Load 1.00 kg |
421 °F @Load 2.21 lb |
50°C/h; ISO 306 |
Polykemi AB SCANMID 6 B12^ NH6 Nylon 6, Flame Retardant, Halogen Free Information provided by Polykemi AB |