Thermal Properties Metric English Comments
Vicat Softening Point 235 °C

@Load 5.00 kg
455 °F

@Load 11.0 lb
120°C/min; ASTM D1525/B, ISO 306/B
EPICHEM Epinyl PA 66 GF25 AU Polyamide 66, 25% Glass, Self extinguishing
Characteristics: 25% glass fibre filled
Vicat Softening Point 235 °C

@Load 5.00 kg
455 °F

@Load 11.0 lb
120°C/min; ASTM D1525/B, ISO 306/B
EPICHEM Epinyl PA 66 Polyamide 66