Vicat Softening Point 80.0 °C

@Load 5.001 kg
176 °F

@Load 11.03 lb
50°C/h; ISO 306
Polykemi AB POLYfill PPC GK8020 Polypropylene Copolymer, Glass Fiber Reinforced
Information provided by Polykemi AB
Vicat Softening Point 80.0 °C

@Load 5.001 kg
176 °F

@Load 11.03 lb
50°C/h; ISO 306
Polykemi AB POLYfill PPH TS15040 D Polypropylene Homopolymer, Mineral Reinforced, Detergent Resistant
Information provided by Polykemi AB
Vicat Softening Point 80.0 °C

@Load 5.001 kg
176 °F

@Load 11.03 lb
50°C/h; ISO 306
Polykemi AB POLYfill PPH K20040 Polypropylene Homopolymer, Mineral Reinforced
Information provided by Polykemi AB
Vicat Softening Point 80.0 °C

@Load 5.001 kg
176 °F

@Load 11.03 lb
50°C/h; ISO 306
Polykemi AB POLYfill PPH K5040 Polypropylene Homopolymer, Mineral Reinforced
Information provided by Polykemi AB
Vicat Softening Point 80.0 °C

@Load 5.001 kg
176 °F

@Load 11.03 lb
50°C/h; ISO 306
Polykemi AB POLYfill PPH K8040 Polypropylene Homopolymer, Mineral Reinforced
Information provided by Polykemi AB
Vicat Softening Point 80.0 °C

@Load 5.001 kg
176 °F

@Load 11.03 lb
50°C/h; ISO 306
Polykemi AB POLYfill PPH Q15030 E10 Polypropylene Homopolymer, Mineral Reinforced, Elastomer Modified
Information provided by Polykemi AB
Vicat Softening Point 80.0 °C

@Load 5.10 kg
176 °F

@Load 11.2 lb
50°C per hour; ISO 306
Total PPC 10641 Polypropylene, Heterophasic Copolymer, Injection Molding
Polypropylene PPC 10641 is a nucleated antistatic heterophasic copolymer with high Melt Flow index of 44 g/10 min.Polypropylene PPC 10641 is characterized by high fluidity with good mechanical prope..
Vicat Softening Point 80.0 °C

@Load 5.10 kg
176 °F

@Load 11.2 lb
50°C per hour; ISO 306
Total PPC 10642 Polypropylene, Heterophasic Copolymer, Injection Molding
Polypropylene PPC 10642 is a nucleated antistatic heterophasic copolymer with high Melt Flow index of 44 g/10 min.Polypropylene PPC 10642 is characterized by high fluidity with good mechanical prope..
Vicat Softening Point 80.0 °C

@Load 5.10 kg
176 °F

@Load 11.2 lb
50°C per hour; ISO 306
Total PPC 12642 Polypropylene, Heterophasic Copolymer, Injection Molding
Polypropylene PPC 12642 is a nucleated antistatic heterophasic copolymer with high Melt Flow index of 70 g/10 min and good mechanical properties.Polypropylene PPC 10641 has been developed for high s..
Vicat Softening Point 80.0 °C

@Load 5.10 kg
176 °F

@Load 11.2 lb
50°C per hour; ISO 306
Total PPM H250 Polypropylene, Homopolymer Medical Grade
Polypropylene PPM H250 is a narrow molecular weight distribution homopolymer with a Melt Flow Index of 25 g/10 min recommended for the manufacture of medical packaging and medical devices, to the ex..
Vicat Softening Point 80.0 °C

@Load 5.10 kg
176 °F

@Load 11.2 lb
50°C per hour; ISO 306
Total PPC 11642 Polypropylene, Heterophasic Copolymer, Injection Molding
Polypropylene PPC 11642 is a nucleated antistatic heterophasic copolymer with high Melt Flow index of 60 g/10 min.Polypropylene PPC 11642 is characterized by high fluidity with good mechanical prope..
Vicat Softening Point 80.0 °C

@Load 5.00 kg
176 °F

@Load 11.0 lb
120°C/hr; ISO 306
Chi Mei Polylac® PA-765 ABS - Flame Retardant
F.R. High Flow
Vicat Softening Point 80.0 °C

@Load 5.001 kg
176 °F

@Load 11.03 lb
50°C/h; ISO 306
Polykemi AB POLYfill PPHC K8030 Polypropylene, Mineral Reinforced
Information provided by Polykemi AB
Vicat Softening Point 80.0 °C

@Load 5.001 kg
176 °F

@Load 11.03 lb
50°C/h; ISO 306
Polykemi AB POLYfill PPHC K8040 Polypropylene, Mineral Reinforced
Information provided by Polykemi AB