Thermal Properties Metric English Comments
Thermal Conductivity 0.0440 W/m-K

@Temperature 20.0 °C
0.305 BTU-in/hr-ft²-°F

@Temperature 68.0 °F
Pyrotek S-1100 Compressible Insulation Board
The Pyrotek S-1100 board is a low density calcium silicate product typically used for back-up insulation in refractory constructions.ApplicationsReduction cell insulation Trough covers Back-up insul..