Thermal Properties Metric English Comments
Thermal Conductivity 0.0778 W/m-K

@Temperature 288 °C
0.540 BTU-in/hr-ft²-°F

@Temperature 550 °F
Duratherm S Silicone Heat Transfer Fluid
Duratherm S - a silicone based heat transfer fluid that is ideally suited for high oxidation or completely exposed systems up to 650°F. Duratherm S is virtually impervious to oxidation and offers s..