Polymer Property : Thermal Conductivity = 0.0840 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.0840 W/m-K

@Temperature 300 °C
0.583 BTU-in/hr-ft²-°F

@Temperature 572 °F
Pyrotek AF-8 Mineral Fiber Paper
Pyrotek's AF-8 Mineral Fiber Paper is a low shot paper used in high temperature gasketing and as an insulating parting agent between refractory and metal work. It is a soft, flexible, clean pa..