Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.0310 W/m-K @Temperature 23.0 °C |
0.215 BTU-in/hr-ft²-°F @Temperature 73.4 °F |
|
Zoltek Panex 35® Carbon Felt Carbon FeltApplications include: Thermal, Corrosive, or Conductive applications |