Thermal Properties Metric English Comments
Thermal Conductivity 0.0813 W/m-K

@Temperature 371 °C
0.564 BTU-in/hr-ft²-°F

@Temperature 700 °F
Paratherm Corporation Paratherm™ HR™ Heat Transfer Fluid
Paratherm HR™ Heat Transfer Fluid is an alkylated-aromatic based heat transfer fluid formulated for closed loop liquid phase heating to 650°F in fired heaters and 675°F in waste heat recovery and..