Thermal Properties Metric English Comments
Thermal Conductivity 0.133 W/m-K

@Temperature 121 °C
0.924 BTU-in/hr-ft²-°F

@Temperature 250 °F
Paratherm Corporation Paratherm™ CR Heat Transfer Fluid
Paratherm CR® heat transfer fluid is a blend of synthetic components formulated to provide superior cooling performance in closed-loop heat-transfer systems operating down to -88°C (-127°F) yet i..
Thermal Conductivity 0.133 W/m-K

@Temperature 204 °C
0.924 BTU-in/hr-ft²-°F

@Temperature 400 °F
Duratherm 600 Paraffinic Heat Transfer Fluid
Duratherm 600 - thermal fluid rated to 600°F it contains the industries most aggressive blend of additives for long, trouble free operation in a variety of applications. Specifically engineered to ..
Thermal Conductivity 0.133 W/m-K

@Temperature 204 °C
0.924 BTU-in/hr-ft²-°F

@Temperature 400 °F
Duratherm 630 Paraffinic Heat Transfer Fluid
Duratherm 630 - rated to 630°F it has the highest rated bulk temperature of petroleum based thermal fluids. Duratherm 630 is engineered for applications requiring high temperature stability (630°F..
Thermal Conductivity 0.133 W/m-K

@Temperature 204 °C
0.924 BTU-in/hr-ft²-°F

@Temperature 400 °F
Duratherm FG Paraffinic Heat Transfer Fluid
Duratherm FG - thermal oil rated to 620°F it is engineered and manufactured to comply with the demands of food grade applications. NSF registered, meets USDA requirements for incidental food contac..