Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.800 - 1.00 W/m-K @Temperature 600 °C |
5.55 - 6.94 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|