Thermal Properties Metric English Comments
Thermal Conductivity 0.147 W/m-K

@Temperature -73.3 °C
1.02 BTU-in/hr-ft²-°F

@Temperature -100 °F
Paratherm Corporation Paratherm™ CR Heat Transfer Fluid
Paratherm CR® heat transfer fluid is a blend of synthetic components formulated to provide superior cooling performance in closed-loop heat-transfer systems operating down to -88°C (-127°F) yet i..
Thermal Conductivity 0.147 W/m-K

@Temperature 65.6 °C
1.02 BTU-in/hr-ft²-°F

@Temperature 150 °F
Paratherm Corporation Paratherm™ LR Heat Transfer Fluid
Paratherm LR™ heat transfer fluid is an aliphatic-hydrocarbon based heat transfer fluid designed for use in closed-loop, liquid phase heating and cooling systems up to 450°F in electric and steam ..