Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.165 W/m-K @Temperature 200 °C |
1.15 BTU-in/hr-ft²-°F @Temperature 392 °F |
ASTM D1674 |
DuPont™ Nomex® Type 994, 125 mil Nominal Thickness Rigid Aromatic Nylon Board Type 994 is a densified, rigid board which has a unique combination of superior resistance to compression, even at elevated temperatures, along with relatively high oil absorption characteristics. T.. |