Polymer Property : Thermal Conductivity = 1.458 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 1.458 W/m-K

@Temperature 900.0 °C
10.12 BTU-in/hr-ft²-°F

@Temperature 1652 °F
Stellar Canada CERAMITE® SFR Wear Resistant Castable
Ceramite is a family of wear resistant castables with a unique combination of high wear resistance, thermal resistance and mechanical strength. Ceramite is produced and supplied to end users world w..