Thermal Properties Metric English Comments
Thermal Conductivity 1.89 - 1.99 W/m-K

@Temperature 1300 °C
13.1 - 13.8 BTU-in/hr-ft²-°F

@Temperature 2370 °F
Gouda Vuurvast VIBRON 150 G RAPID Dense Vibrating Refractory Castable
Description: Vibron 150 G Rapid is a low cement castable based on sintered South-American bauxite. Because of special additives this material is suited for direct contact with liquid aluminum and al..
Thermal Conductivity 1.89 W/m-K

@Temperature 1093 °C
13.1 BTU-in/hr-ft²-°F

@Temperature 1999 °F
Pyrotek Pyrocast ALF3 Low Cement Refractory Castable
Pyrocast ALF3 is a low cement castable with a high-purity mullite base. It is suited for applications exposed to high erosion or aggressive alloys and/or atmospheres.ApplicationsAluminum melting an..