Thermal Conductivity 146.8 W/m-K

@Temperature 25.0 °C
1019 BTU-in/hr-ft²-°F

@Temperature 77.0 °F
Osprey Metals CE17M Al-Si Controlled Expansion Alloy
Al-27%Si+ controlled expansion alloy manufactured and patented by Osprey Metals Ltd.Information provided to MatWeb by Osprey Metals.