Thermal Conductivity 15.1 W/m-K

@Temperature 93.0 °C
105 BTU-in/hr-ft²-°F

@Temperature 199 °F
AK Steel PH 15-7 Mo® Precipitation Hardening Stainless Steel, Condition RH 950
AK Steel 15-7 Mo® provides high strength and hardness, good corrosion resistance and minimum distortion on heat treatment. It is easily formed in the annealed condition and develops effective bala..
Thermal Conductivity 15.1 W/m-K

@Temperature 93.0 °C
105 BTU-in/hr-ft²-°F

@Temperature 199 °F
AK Steel PH 15-7 Mo® Precipitation Hardening Stainless Steel, Condition TH 1050
AK Steel 15-7 Mo® provides high strength and hardness, good corrosion resistance and minimum distortion on heat treatment. It is easily formed in the annealed condition and develops effective bala..