Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 108.4 W/m-K @Temperature 400 °C |
752.3 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
PEAK Werkstoff DISPAL S250 Aluminum Alloy, AlSi20Fe5Ni2, Condition F Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational.. |