Thermal Conductivity 12.22 W/m-K

@Temperature 50.0 °C
84.81 BTU-in/hr-ft²-°F

@Temperature 122 °F
Carpenter Gall-Tough® Stainless
Data provided by Carpenter Technology Corporation.6.4 mm diameter tensile specimens from center of 25.4 mm diameter bar annealed 1066°C 1 hour, water quenched, and ground.Threshold Galling Stress 1..