Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 2.00 W/m-K @Temperature 650 °C |
13.9 BTU-in/hr-ft²-°F @Temperature 1200 °F |
|
Gouda Vuurvast AC 80-10 Dense Refractory Brick Description: This bauxite base brick shows, due to the addition of CR2O3, a very good slag resistance.Remarks: This data represents average values, obtained from samples that were cut from standard .. |
|||
Thermal Conductivity | 2.00 W/m-K @Temperature 650 °C |
13.9 BTU-in/hr-ft²-°F @Temperature 1200 °F |
|
Gouda Vuurvast AC 80-5 Dense Refractory Brick Description: This Cr2O3 containing brick shows a good slag and abrasion resistance. Application in ZnO furnaces.Remarks: This data represents average values, obtained from samples that were cut from.. |
|||
Thermal Conductivity | 2.00 W/m-K @Temperature 650 °C |
13.9 BTU-in/hr-ft²-°F @Temperature 1200 °F |
|
Gouda Vuurvast AK 70 K Dense Refractory Brick Description: A high quality andalusite/corundum brick with a mullite bond with a very good volume stability. Also good slag- and thermal shock resistance.Remarks: This data represents average values.. |
|||
Thermal Conductivity | 2.00 W/m-K @Temperature 650 °C |
13.9 BTU-in/hr-ft²-°F @Temperature 1200 °F |
|
Gouda Vuurvast AK 70 M Dense Refractory Brick Description: This mullite brick is characterized by a very good thermal shock resistance, a high resistance against slag penetration and a high strength.Remarks: This data represents average values,.. |
|||
Thermal Conductivity | 2.00 - 2.20 W/m-K @Temperature 100 °C |
13.9 - 15.3 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast CURASBOND 85 Moldable Refractory Material Description: Curasbond 85 is a pouring repairmass, characterized by excellent resistance to aluminum and rapid hardening. The product is supplied in two components: a dry powder and a liquid. It can.. |
|||
Thermal Conductivity | 2.00 W/m-K @Temperature 100 °C |
13.9 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Kuraray Vectran® HT 1500/300 LCP Fiber  is a high-performance multifilament yarn spun from liquid crystal polymer (LCP).  fiber exhibits exceptional strength and rigidity. Pound for pound  fiber is five times stronger than steel an.. |
|||
Thermal Conductivity | 2.00 W/m-K @Temperature 650 °C |
13.9 BTU-in/hr-ft²-°F @Temperature 1200 °F |
|
Gouda Vuurvast AK 70 A Dense Refractory Brick Description: This brick is made of a high quality bauxite. Application: transition zone of rotary cement kiln.Remarks: This data represents average values, obtained from samples that were cut from s.. |
|||
Thermal Conductivity | 2.00 W/m-K @Temperature 650 °C |
13.9 BTU-in/hr-ft²-°F @Temperature 1200 °F |
|
Gouda Vuurvast AK 70 KP Dense Refractory Brick Description: A high quality phosphate bonded andalusite/corundum brick with very good volume stability. Also good slag resistance and thermal shock resistance. Remarks: This data represents average .. |
|||
Thermal Conductivity | 2.00 W/m-K @Temperature 1100 °C |
13.9 BTU-in/hr-ft²-°F @Temperature 2010 °F |
|
Gouda Vuurvast AK 85 KM Dense Refractory Brick Description: This brick based on mullite and corundum, is characterized by a very low porosity, high slag resistance, low creep and very good thermal shock resistance.Remarks: This data represents a.. |
|||
Thermal Conductivity | 2.00 - 2.20 W/m-K @Temperature 1600 °C |
13.9 - 15.3 BTU-in/hr-ft²-°F @Temperature 2910 °F |
|
Gouda Vuurvast FLUCON 180 Dense Self Flowing Refractory Castable Description: Flucon 180 is a self flowing castable based on white fused Alumina. This castable is applied at severe thermal conditions and or severe slag attack.Remarks: These values apply to cast p.. |