Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 130.9 W/m-K @Temperature 100 °C |
908.4 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
PEAK Werkstoff DISPAL S693 Aluminum Alloy, AlCu5Ti, Condition T6 High stiffness and elongation at rupture. Property data for Condition T6 (Quench in water at RT).Information provided by PEAK Werkstoff GmbH |
|||
Thermal Conductivity | 130.9 W/m-K @Temperature 100 °C |
908.4 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
PEAK Werkstoff DISPAL S693 Aluminum Alloy, AlCu5Ti, Condition T4 High stiffness and elongation at rupture. Property data for Condition T4 (Quench in water at RT).Information provided by PEAK Werkstoff GmbH |