Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Thermal Conductivity = 14.4 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 14.4 W/m-K

@Temperature 200 °C
99.9 BTU-in/hr-ft²-°F

@Temperature 392 °F
Haynes Hastelloy® G-30® alloy, all-weld metal, GTAW weld 3.2 mm diameter filler wire
HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid..
Thermal Conductivity 14.4 W/m-K

@Temperature 200 °C
99.9 BTU-in/hr-ft²-°F

@Temperature 392 °F
Haynes Hastelloy® G-30® alloy, mill annealed
HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid..
Thermal Conductivity 14.4 W/m-K

@Temperature 200 °C
99.9 BTU-in/hr-ft²-°F

@Temperature 392 °F
Haynes Hastelloy® G-30® alloy, 12.7 mm (1/2 in.) thick plate, GMAW spray weld 1.1 mm diameter filler wire
HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid..
Thermal Conductivity 14.4 W/m-K

@Temperature 200 °C
99.9 BTU-in/hr-ft²-°F

@Temperature 392 °F
Haynes Hastelloy® G-30® alloy, 12.7 mm (1/2 in.) thick plate, GTAW weld 3.2 mm diameter filler wire
HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid..
Thermal Conductivity 14.4 W/m-K

@Temperature 200 °C
99.9 BTU-in/hr-ft²-°F

@Temperature 392 °F
Haynes Hastelloy® G-30® alloy, 25.4 mm thick bar
HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid..
Thermal Conductivity 14.4 W/m-K

@Temperature 200 °C
99.9 BTU-in/hr-ft²-°F

@Temperature 392 °F
Haynes Hastelloy® G-30® alloy, 3.2 mm thick sheet
HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid..
Thermal Conductivity 14.4 W/m-K

@Temperature 200 °C
99.9 BTU-in/hr-ft²-°F

@Temperature 392 °F
Haynes Hastelloy® G-30® alloy, 3.2 mm thick sheet, GTAW weld
HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid..
Thermal Conductivity 14.4 W/m-K

@Temperature 200 °C
99.9 BTU-in/hr-ft²-°F

@Temperature 392 °F
Haynes Hastelloy® G-30® alloy, 30% cold rolled
HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid..
Thermal Conductivity 14.4 W/m-K

@Temperature 200 °C
99.9 BTU-in/hr-ft²-°F

@Temperature 392 °F
Haynes Hastelloy® G-30® alloy, 50% cold rolled
HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid..
Thermal Conductivity 14.4 W/m-K

@Temperature 200 °C
99.9 BTU-in/hr-ft²-°F

@Temperature 392 °F
Haynes Hastelloy® G-30® alloy, 50% cold rolled and 1 hour at 500°C, air cooled
HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid..
Thermal Conductivity 14.4 W/m-K

@Temperature 200 °C
99.9 BTU-in/hr-ft²-°F

@Temperature 392 °F
Haynes Hastelloy® G-30® alloy, 50% cold rolled and 5000 hours at 500°C, air cooled
HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid..
Thermal Conductivity 14.4 W/m-K

@Temperature 200 °C
99.9 BTU-in/hr-ft²-°F

@Temperature 392 °F
Haynes Hastelloy® G-30® alloy, 6.4 mm thick plate
HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid..
Thermal Conductivity 14.4 W/m-K

@Temperature 200 °C
99.9 BTU-in/hr-ft²-°F

@Temperature 392 °F
Haynes Hastelloy® G-30® alloy, 9.5 mm thick plate
HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid..
Thermal Conductivity 14.4 W/m-K

@Temperature 200 °C
99.9 BTU-in/hr-ft²-°F

@Temperature 392 °F
Haynes Hastelloy® G-30® alloy, all-weld metal, GMAW weld 1.1 mm diameter filler wire
HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid..
Thermal Conductivity 14.4 W/m-K

@Temperature 200 °C
99.9 BTU-in/hr-ft²-°F

@Temperature 392 °F
Haynes Hastelloy® G-30® alloy, plate and bar
HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid..
Thermal Conductivity 14.4 W/m-K

@Temperature 20.0 °C
99.9 BTU-in/hr-ft²-°F

@Temperature 68.0 °F
Hardened Condition
Bohler-Uddeholm BÖHLER W302 SUPERIOR® Premium H13 Tool Steel
A premium grade H13 hot work tool steel featuring:Very good toughness properties meeting the requirements of NADCA 207-97, and the superior quality levels of NADCA 207-2003Very good heat checking re..
Thermal Conductivity 14.4 W/m-K

@Temperature 200 °C
99.9 BTU-in/hr-ft²-°F

@Temperature 392 °F
Haynes Hastelloy® G-30® alloy, 0.71 mm thick sheet
HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxidizin..
Thermal Conductivity 14.4 W/m-K

@Temperature 200 °C
99.9 BTU-in/hr-ft²-°F

@Temperature 392 °F
Haynes Hastelloy® G-30® alloy, 10% cold rolled
HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxidizin..
Thermal Conductivity 14.4 W/m-K

@Temperature 200 °C
99.9 BTU-in/hr-ft²-°F

@Temperature 392 °F
Haynes Hastelloy® G-30® alloy, 12.7 mm (1/2 in.) thick plate, GTAW short arc weld 1.1 mm diameter filler wire
HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxidizin..
Thermal Conductivity 14.4 W/m-K

@Temperature 200 °C
99.9 BTU-in/hr-ft²-°F

@Temperature 392 °F
Haynes Hastelloy® G-30® alloy, 19.1 mm thick plate
HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxidizin..
Thermal Conductivity 14.4 W/m-K

@Temperature 200 °C
99.9 BTU-in/hr-ft²-°F

@Temperature 392 °F
Haynes Hastelloy® G-30® alloy, 31.8 mm thick plate
HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxidizin..
Thermal Conductivity 14.4 W/m-K

@Temperature 200 °C
99.9 BTU-in/hr-ft²-°F

@Temperature 392 °F
Haynes Hastelloy® G-30® alloy, 12.7 mm (1/2 in.) thick plate
HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxidizin..
Copyright © lookpolymers.com All Rights Reserved