Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Thermal Conductivity = 14.8 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 14.8 W/m-K

@Temperature 316 °C
103 BTU-in/hr-ft²-°F

@Temperature 601 °F
Annealed
Special Metals INCONEL® alloy 783 Ni-Co-Fe Alloy
The newest of the high-performance superalloys invented by Special Metals Corporation, INCONEL® alloy 783 (UNS R30783/US Patent 5,478,417), is an oxidation-resistant, low expansion, nickel-cobalt..
Thermal Conductivity 14.8 W/m-K

@Temperature 200 °C
103 BTU-in/hr-ft²-°F

@Temperature 392 °F
Carpenter 20-Mo6® Stainless Steel, Plate
Data provided by Carpenter Technology Corporation.This is an austenitic stainless steel which is resistant to corrosion in hot chloride environments with low pH. It has good resistance to pitting, ..
Thermal Conductivity 14.8 W/m-K

@Temperature 200 °C
103 BTU-in/hr-ft²-°F

@Temperature 392 °F
Carpenter 20-Mo6® Stainless Steel, Strip
Data provided by Carpenter Technology Corporation.This is an austenitic stainless steel which is resistant to corrosion in hot chloride environments with low pH. It has good resistance to pitting, ..
Thermal Conductivity 14.8 W/m-K

@Temperature 200 °C
103 BTU-in/hr-ft²-°F

@Temperature 392 °F
Carpenter 20-Mo6® Stainless Steel, Tensile Properties at 93°C
Data provided by Carpenter Technology Corporation.This is an austenitic stainless steel which is resistant to corrosion in hot chloride environments with low pH. It has good resistance to pitting, ..