Polymer Property : Thermal Conductivity = 141 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 20.3 W/m-K

@Temperature 500 °C
141 BTU-in/hr-ft²-°F

@Temperature 932 °F
Haynes Hastelloy® G-30® alloy, all-weld metal, GTAW weld 3.2 mm diameter filler wire
HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid..
Thermal Conductivity 20.3 W/m-K

@Temperature 500 °C
141 BTU-in/hr-ft²-°F

@Temperature 932 °F
Haynes Hastelloy® G-30® alloy, mill annealed
HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid..
Thermal Conductivity 20.3 W/m-K

@Temperature 500 °C
141 BTU-in/hr-ft²-°F

@Temperature 932 °F
Haynes Hastelloy® G-30® alloy, 12.7 mm (1/2 in.) thick plate, GMAW spray weld 1.1 mm diameter filler wire
HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid..
Thermal Conductivity 20.3 W/m-K

@Temperature 500 °C
141 BTU-in/hr-ft²-°F

@Temperature 932 °F
Haynes Hastelloy® G-30® alloy, 12.7 mm (1/2 in.) thick plate, GTAW weld 3.2 mm diameter filler wire
HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid..
Thermal Conductivity 20.3 W/m-K

@Temperature 500 °C
141 BTU-in/hr-ft²-°F

@Temperature 932 °F
Haynes Hastelloy® G-30® alloy, 25.4 mm thick bar
HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid..
Thermal Conductivity 20.3 W/m-K

@Temperature 500 °C
141 BTU-in/hr-ft²-°F

@Temperature 932 °F
Haynes Hastelloy® G-30® alloy, 3.2 mm thick sheet
HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid..
Thermal Conductivity 20.3 W/m-K

@Temperature 500 °C
141 BTU-in/hr-ft²-°F

@Temperature 932 °F
Haynes Hastelloy® G-30® alloy, 3.2 mm thick sheet, GTAW weld
HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid..
Thermal Conductivity 20.3 W/m-K

@Temperature 500 °C
141 BTU-in/hr-ft²-°F

@Temperature 932 °F
Haynes Hastelloy® G-30® alloy, 30% cold rolled
HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid..
Thermal Conductivity 20.3 W/m-K

@Temperature 500 °C
141 BTU-in/hr-ft²-°F

@Temperature 932 °F
Haynes Hastelloy® G-30® alloy, 50% cold rolled
HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid..
Thermal Conductivity 20.3 W/m-K

@Temperature 500 °C
141 BTU-in/hr-ft²-°F

@Temperature 932 °F
Haynes Hastelloy® G-30® alloy, 50% cold rolled and 1 hour at 500°C, air cooled
HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid..
Thermal Conductivity 20.3 W/m-K

@Temperature 500 °C
141 BTU-in/hr-ft²-°F

@Temperature 932 °F
Haynes Hastelloy® G-30® alloy, 50% cold rolled and 5000 hours at 500°C, air cooled
HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid..
Thermal Conductivity 20.3 W/m-K

@Temperature 500 °C
141 BTU-in/hr-ft²-°F

@Temperature 932 °F
Haynes Hastelloy® G-30® alloy, 6.4 mm thick plate
HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid..
Thermal Conductivity 20.3 W/m-K

@Temperature 500 °C
141 BTU-in/hr-ft²-°F

@Temperature 932 °F
Haynes Hastelloy® G-30® alloy, 9.5 mm thick plate
HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid..
Thermal Conductivity 20.3 W/m-K

@Temperature 500 °C
141 BTU-in/hr-ft²-°F

@Temperature 932 °F
Haynes Hastelloy® G-30® alloy, all-weld metal, GMAW weld 1.1 mm diameter filler wire
HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid..
Thermal Conductivity 20.3 W/m-K

@Temperature 500 °C
141 BTU-in/hr-ft²-°F

@Temperature 932 °F
Haynes Hastelloy® G-30® alloy, plate and bar
HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid..
Thermal Conductivity 20.3 W/m-K

@Temperature 482 °C
141 BTU-in/hr-ft²-°F

@Temperature 900 °F
Crucible Steel XM-19 Stainless Steel
Crucible XM-19 Stainless is a nitrogen strengthened, low carbon, austenitic, stainless steel that provides good corrosion resistance in combination with high strength. The alloy has better corrosio..
Thermal Conductivity 20.3 W/m-K

@Temperature 500 °C
141 BTU-in/hr-ft²-°F

@Temperature 932 °F
Haynes Hastelloy® G-30® alloy, 0.71 mm thick sheet
HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxidizin..
Thermal Conductivity 20.3 W/m-K

@Temperature 500 °C
141 BTU-in/hr-ft²-°F

@Temperature 932 °F
Haynes Hastelloy® G-30® alloy, 10% cold rolled
HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxidizin..
Thermal Conductivity 20.3 W/m-K

@Temperature 500 °C
141 BTU-in/hr-ft²-°F

@Temperature 932 °F
Haynes Hastelloy® G-30® alloy, 12.7 mm (1/2 in.) thick plate, GTAW short arc weld 1.1 mm diameter filler wire
HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxidizin..
Thermal Conductivity 20.3 W/m-K

@Temperature 500 °C
141 BTU-in/hr-ft²-°F

@Temperature 932 °F
Haynes Hastelloy® G-30® alloy, 19.1 mm thick plate
HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxidizin..
Thermal Conductivity 20.3 W/m-K

@Temperature 500 °C
141 BTU-in/hr-ft²-°F

@Temperature 932 °F
Haynes Hastelloy® G-30® alloy, 31.8 mm thick plate
HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxidizin..
Thermal Conductivity 20.3 W/m-K

@Temperature 500 °C
141 BTU-in/hr-ft²-°F

@Temperature 932 °F
Haynes Hastelloy® G-30® alloy, 12.7 mm (1/2 in.) thick plate
HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxidizin..