Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 22.4 W/m-K @Temperature 25.0 °C |
155 BTU-in/hr-ft²-°F @Temperature 77.0 °F |
|
International Mold Steel Daido DRM1 Matrix High-Speed Steel This tough matrix type high speed tool steel features high hardness and high tough Matrix type high speed tool steel vastly surpasses hot work die steels. DRM1 improves hot and warm die life by its .. |
|||
Thermal Conductivity | 22.4 W/m-K @Temperature 600 °C |
155 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Haynes Hastelloy® C-22HS™ Nickel Alloy Gas Tungsten Arc Welded (GTAW) All Weld Cruciform Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou.. |
|||
Thermal Conductivity | 22.4 W/m-K @Temperature 600 °C |
155 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Haynes Hastelloy® C-22HS™ Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou.. |
|||
Thermal Conductivity | 22.4 W/m-K @Temperature 600 °C |
155 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Haynes Hastelloy® C-22HS™ Nickel Alloy Gas Tungsten Arc Welded (GTAW) Sheet Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou.. |
|||
Thermal Conductivity | 22.4 W/m-K @Temperature 600 °C |
155 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Haynes Hastelloy® C-22HS™ Nickel Alloy Plate and Bar, Hot-rolled, Solution Annealed Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou.. |
|||
Thermal Conductivity | 22.4 W/m-K @Temperature 600 °C |
155 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Haynes Hastelloy® C-22HS™ Nickel Alloy Sheet, Cold-rolled, Solution Annealed Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou.. |
|||
Thermal Conductivity | 22.4 W/m-K @Temperature 600 °C |
155 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Haynes Hastelloy® C-22HS™ Nickel Alloy Sheet, Cold-rolled, Solution Annealed, Age-hardened Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou.. |
|||
Thermal Conductivity | 22.4 W/m-K @Temperature 600 °C |
155 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Haynes Hastelloy® C-22HS™ Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) All Weld Cruciform Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou.. |
|||
Thermal Conductivity | 22.4 W/m-K @Temperature 600 °C |
155 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Haynes Hastelloy® C-22HS™ Nickel Alloy Plate and Bar, Hot-rolled, Solution Annealed, Age-hardened Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately doubl.. |
|||
Thermal Conductivity | 22.4 W/m-K @Temperature 600 °C |
155 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Haynes Hastelloy® C-22HS™ Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) Plate Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately doubl.. |
|||
Thermal Conductivity | 22.3 W/m-K @Temperature 504 °C |
155 BTU-in/hr-ft²-°F @Temperature 940 °F |
|
Schmolz + Bickenbach Formadur® PH X Superclean Plastic Mold Steel Description: Formadur® PH X Superclean is a corrosion-resistant, martensitic precipitation hardened stainless steelCharacteristics: Excellent resistance to corrosion; Excellent polishability; Excel.. |