Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 22.8 W/m-K @Temperature 700 °C |
158 BTU-in/hr-ft²-°F @Temperature 1290 °F |
|
Haynes Hastelloy® X alloy, sheet Solid-solution-strengthened with very good high-temperature strength and very good resistance to oxidizing environments up to about 1095°C, and good carburization resistance. Applications includ.. |
|||
Thermal Conductivity | 22.7 W/m-K @Temperature 800 °C |
158 BTU-in/hr-ft²-°F @Temperature 1470 °F |
|
Haynes Waspaloy™ alloy, sheet Age-hardenable superalloy with very good strength at temperatures up 980°C (1800°F), can be cold-formed in the annealed condition, may also be hot formed at 1040°C (1900°F) and above, go.. |
|||
Thermal Conductivity | 22.7 W/m-K @Temperature 800 °C |
158 BTU-in/hr-ft²-°F @Temperature 1470 °F |
|
Haynes X-750 Nickel Alloy Sheet and Strip (AMS 5598, UNS N07750) Haynes X-750 (UNS No. N07750) alloy is an age-hardenable, nickel-base superalloy with very good strength at temperatures up to about 1600°F (870°C). It is widely used as a wrought material for.. |
|||
Thermal Conductivity | 22.7 W/m-K @Temperature 600 °C |
158 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Haynes 75 Nickel Alloy Sheet, Annealed at 1925°F (1050°C) Haynes alloy 75 is a solution-strengthened nickel-chromium alloy with moderate strength to 1200°F (650°C). It is principally used in low stress elevated temperature applications requiring reas.. |
|||
Thermal Conductivity | 22.8 W/m-K @Temperature 500 °C |
158 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
AK Steel 13-4 SR® Ferritic Stainless Steel AK Steel 13-4 SR Stainless Steel is a ductile weldable ferritic with 13% Cr and 3.75% Al. The high aluminum content results in a base alloy with high electrical resistivity. It is intended for use w.. |
|||
Thermal Conductivity | 22.8 W/m-K @Temperature 871 °C |
158 BTU-in/hr-ft²-°F @Temperature 1600 °F |
|
ATI Allegheny Ludlum AL 625HP™ Stainless Steel Nickel-based superalloy. Characteristics:exceptional fatigue resistance, excellent resistance to oxidation and corrosion, outstanding strength and toughness over a range of temperatures from cryogen.. |
|||
Thermal Conductivity | 22.7 W/m-K @Temperature 200 °C |
158 BTU-in/hr-ft²-°F @Temperature 392 °F |
|
QuesTek® Innovations Ferrium® S53® Corrosion Resistant High Strength Steel for Aerospace Structural Applications Description: Ferrium® S53® is a corrosion resistant ultra high-strength steel for structural aerospace applications. Ferrium® S53® was designed to provide mechanical properties equal to, or bett.. |