Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 16.2 W/m-K @Temperature 200 °C |
112 BTU-in/hr-ft²-°F @Temperature 392 °F |
Annealed Condition |
Bohler-Uddeholm BÖHLER W302 SUPERIOR® Premium H13 Tool Steel A premium grade H13 hot work tool steel featuring:Very good toughness properties meeting the requirements of NADCA 207-97, and the superior quality levels of NADCA 207-2003Very good heat checking re.. |
|||
Thermal Conductivity | 16.2 W/m-K @Temperature 100 °C |
112 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
AK Steel 201 Austenitic Stainless steel AK Steel 210 was developed originally to conserve nickel. It provides properties similar to Type 301 and can be used in most applications for Type 301. This alloy is non-magnetic in the annealed c.. |
|||
Thermal Conductivity | 16.2 W/m-K @Temperature 100 °C |
112 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
AK Steel 201LN Austenitic Stainless steel AK Steel 210 was developed originally to conserve nickel. It provides properties similar to Type 301 and can be used in most applications for Type 301. This alloy is non-magnetic in the annealed c.. |
|||
Thermal Conductivity | 16.2 W/m-K @Temperature 100 °C |
112 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
AK Steel 301 Austenitic Stainless steel AK Steel 301 provides high strength and good ductility when cold worked. It is a modification of AK Steel 302 to increase the cold work-hardening range, to permit higher tensile strengths to be ach.. |
|||
Thermal Conductivity | 16.2 W/m-K @Temperature 100 °C |
112 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
AK Steel 304 Austenitic Stainless steel AK Steel 304 is a variation of the basic 18-8 grade, Type 302. Lower carbon, in Type 304, minimizes chromium carbide precipitation due to welding and its susceptibility to intergranular corrosion. .. |
|||
Thermal Conductivity | 16.2 W/m-K @Temperature 100 °C |
112 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
AK Steel 304L Austenitic Stainless steel AK Steel 304L is an extra low-carbon variation of Type 304, that eliminates carbide precipitation due to welding. AK Steel 304L can be used in the "as-welded" condition, even in severe corrosive co.. |
|||
Thermal Conductivity | 16.2 W/m-K @Temperature 100 °C |
112 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
AK Steel 305 Austenitic Stainless steel AK Steel 305 can be spun and deep drawn more easily due to an increased nickel content that decreases work hardening. It is non-magnetic and cannot be hardened by heat treatment. Typical uses incl.. |
|||
Thermal Conductivity | 16.2 W/m-K @Temperature 100 °C |
112 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
AK Steel 316L Austenitic Stainless steel AK Steel 316L is an extra-low carbon version of AK Steel 316 that minimizes harmful carbide precipitation due to welding.Information provided by AK Steel |
|||
Thermal Conductivity | 16.2 W/m-K @Temperature 100 °C |
112 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
AK Steel 316 Austenitic Stainless steel AK Steel 316 contains molybdenum. This addition increases general corrosion resistance, improves resistance to pitting from chloride ion solutions, and provides increased strength at elevated tempe.. |