Thermal Properties Metric English Comments
Thermal Conductivity 16.25 W/m-K

@Temperature 93.3 °C
112.8 BTU-in/hr-ft²-°F

@Temperature 200 °F
Crucible Steel 303 Plus Chromium-Nickel Steel
Crucible 303 Plus is a non-hardenable austenitic chromium-nickel steel to which elements have been added to improve machinability and non-galling characteristics. Better machinability than that of..
Thermal Conductivity 16.25 W/m-K

@Temperature 93.3 °C
112.8 BTU-in/hr-ft²-°F

@Temperature 200 °F
Crucible Steel 303 SE Chromium-Nickel Steel
Crucible 303 SE is a non-hardenable austenitic chromium-nickel steel to which selenium has been added to improve machinability and non-galling characteristics. This grade is non-magnetic in the anne..
Thermal Conductivity 16.25 W/m-K

@Temperature 93.3 °C
112.8 BTU-in/hr-ft²-°F

@Temperature 200 °F
Crucible Steel 304L Chromium-Nickel Steel
Crucible 304L is a non-hardenable, low carbon austenitic chromium-nickel steel designed for special applications. It is particularly suitable for applications requiring welding operations where it i..