Polymer Property : Thermal Conductivity = 16.87 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 16.87 W/m-K

@Temperature 149 °C
117.1 BTU-in/hr-ft²-°F

@Temperature 300 °F
AK Steel 17-7 PH® Precipitation Hardening Stainless Steel, Condition RH 950
AK Steel 17-7 PH® provides high strength and hardness, excellent fatigue properties, good corrosion resistance, good formability, and minimum distortion upon heat treatment. This alloy provides va..
Thermal Conductivity 16.87 W/m-K

@Temperature 149 °C
117.1 BTU-in/hr-ft²-°F

@Temperature 300 °F
AK Steel 17-7 PH® Precipitation Hardening Stainless Steel, Condition TH 1050
AK Steel 17-7 PH® provides high strength and hardness, excellent fatigue properties, good corrosion resistance, good formability, and minimum distortion upon heat treatment. This alloy provides va..