Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 16.9 W/m-K @Temperature 400 °C |
117 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Haynes Hastelloy® X alloy, sheet Solid-solution-strengthened with very good high-temperature strength and very good resistance to oxidizing environments up to about 1095°C, and good carburization resistance. Applications includ.. |
|||
Thermal Conductivity | 16.9 W/m-K @Temperature 400 °C |
117 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Haynes X-750 Nickel Alloy Sheet and Strip (AMS 5598, UNS N07750) Haynes X-750 (UNS No. N07750) alloy is an age-hardenable, nickel-base superalloy with very good strength at temperatures up to about 1600°F (870°C). It is widely used as a wrought material for.. |
|||
Thermal Conductivity | 16.9 W/m-K @Temperature 600 °C |
117 BTU-in/hr-ft²-°F @Temperature 1110 °F |
Hardened Condition |
Bohler-Uddeholm BÖHLER W302 SUPERIOR® Premium H13 Tool Steel A premium grade H13 hot work tool steel featuring:Very good toughness properties meeting the requirements of NADCA 207-97, and the superior quality levels of NADCA 207-2003Very good heat checking re.. |