Thermal Properties Metric English Comments
Thermal Conductivity 18.3 W/m-K

@Temperature 600 °C
127 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Haynes 625SQ® Nickel Alloy Sheet
Haynes 625SQ alloy is a solid-solution strengthened superalloy. It is a modification of Haynes 625 alloy designed to enhance resistance to fatigue at temperatures up to approximately 1200°F (649Â..