Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 18.4 W/m-K

@Temperature 500 °C
128 BTU-in/hr-ft²-°F

@Temperature 932 °F
Haynes Hastelloy® C-4 alloy, all-weld metal, as welded, GTAW
Nickel-chromium-molybdenum alloy with outstanding high-temperature stability as evidenced by high ductility and corrosion resistance even after aging in the 1200 to 1900°F (649 to 1038°C) rang..
Thermal Conductivity 18.4 W/m-K

@Temperature 500 °C
128 BTU-in/hr-ft²-°F

@Temperature 932 °F
Haynes Hastelloy® C-4 alloy, welded plate 12.7 mm (1/2 in.) thick, aged 1000 hours at 649°C (1200°F)
Nickel-chromium-molybdenum alloy with outstanding high-temperature stability as evidenced by high ductility and corrosion resistance even after aging in the 1200 to 1900°F (649 to 1038°C) rang..
Thermal Conductivity 18.4 W/m-K

@Temperature 25.0 °C
128 BTU-in/hr-ft²-°F

@Temperature 77.0 °F
COI Ceramics Nicalon™ HI Type S SiC Ceramic Fiber
Description: A stoichiometric beta-SiC fiber manufactured near-oxygen-free using decarbonization pyrolysis and electron-beam curing. It has higher modulus, creep resistance and oxidation resistance ..
Thermal Conductivity 18.4 W/m-K

@Temperature 500 °C
128 BTU-in/hr-ft²-°F

@Temperature 932 °F
Haynes Hastelloy® C-4 alloy, welded plate 12.7 mm (1/2 in.) thick, aged 10 hours at 649°C (1200°F)
Nickel-chromium-molybdenum alloy with outstanding high-temperature stability as evidenced by high ductility and corrosion resistance even after aging in the 1200 to 1900°F (649 to 1038°C) range. T..
Thermal Conductivity 18.4 W/m-K

@Temperature 500 °C
128 BTU-in/hr-ft²-°F

@Temperature 932 °F
Haynes Hastelloy® C-4 alloy, welded plate 12.7 mm (1/2 in.) thick, GTAW
Nickel-chromium-molybdenum alloy with outstanding high-temperature stability as evidenced by high ductility and corrosion resistance even after aging in the 1200 to 1900°F (649 to 1038°C) range. T..