Thermal Properties Metric English Comments
Thermal Conductivity 18.552 W/m-K

@Temperature 300 °C
128.75 BTU-in/hr-ft²-°F

@Temperature 572 °F
Special Metals INCOLOY® alloy 832 Stainless Steel
INCOLOY® alloy 832 is a low cost stainless steel developed specifically for domestic and industrial sheathed heater applications. With specific chemistry additions to ensure satisfactory formula..