Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 26.0 W/m-K @Temperature 700 °C |
180 BTU-in/hr-ft²-°F @Temperature 1290 °F |
|
International Mold Steel Daido DRM3 Matrix High-Speed Steel This conventional grade MH88 has been improved to DRM3. High hardness and tough DRM3 with excellent hardenability is suitable for high precision cold working tools.Information provided by Internatio.. |
|||
Thermal Conductivity | 26.0 W/m-K @Temperature 20.0 °C |
180 BTU-in/hr-ft²-°F @Temperature 68.0 °F |
|
International Mold Steel DH31-EX Die Cast & Forging Steel DH31-EX is a hot working die steel with the best balance of strength and toughness showing the comparable softening resistance to SKD7 and twice hardenability as that of SKD61.Information provided b.. |
|||
Thermal Conductivity | 25.9 W/m-K @Temperature 760 °C |
180 BTU-in/hr-ft²-°F @Temperature 1400 °F |
|
Latrobe LSSâ„¢ H14 Tool Steel (ASTM H14) TLS H14 tool steel is a 5%-chromium hot work steel to which tungsten has been added for improved high-temperature properties and heat resistance. It is a deep-hardening, airhardening
steel that exh.. |
|||
Thermal Conductivity | 26.0 W/m-K @Temperature 20.0 °C |
180 BTU-in/hr-ft²-°F @Temperature 68.0 °F |
|
CoorsTek ADS-96R 96% Alumina Thick Film Substrate This high-purity material ensures strong, reliable performance for ceramic substrate application. Applications: thick films and lasers |
|||
Thermal Conductivity | 26.0 W/m-K @Temperature 20.0 °C |
180 BTU-in/hr-ft²-°F @Temperature 68.0 °F |
|
CoorsTek ADSR-96R DuraStrate™ 96% Alumina Thick Film Applications: thick films and lasers |
|||
Thermal Conductivity | 26.0 W/m-K @Temperature 95.0 °C |
180 BTU-in/hr-ft²-°F @Temperature 203 °F |
|
Crucible Steel Nu-Die® V (AISI H13) Hot Work Tool Steel Nu-Die® V (AISI H13) has been the most popular, and perhaps the most versatile hot work tool steel available for many years. It provides a good balance of toughness, heat check resistance and tempe.. |
|||
Thermal Conductivity | 26.0 W/m-K @Temperature 95.0 °C |
180 BTU-in/hr-ft²-°F @Temperature 203 °F |
|
Crucible Steel Nu-Die® XL (Premium Quality AISI H13) Tool Steel Nu-Die XL (AISI H13) is a premium version of H13 tool steel manufactured, tested and certified to meet stringent die casting industry specifications issued by NADCA, Chrysler and others. It offers b.. |
|||
Thermal Conductivity | 26.0 W/m-K @Temperature 20.0 °C |
180 BTU-in/hr-ft²-°F @Temperature 68.0 °F |
hardened to 62 HRC |
Bohler-Uddeholm AISI A2 Cold Work Tool Steel Description: AISI A2 is an air- or oil hardening chromiummolybdenum-vanadium alloyed tool steel characterized byAISI A2 is characterized by: Good machinability High stability after hardening High c.. |
|||
Thermal Conductivity | 26.0 W/m-K @Temperature 20.0 °C |
180 BTU-in/hr-ft²-°F @Temperature 68.0 °F |
|
Assab Steels VANADIS 4 Cold Work Steel VANADIS 4 is a chromium-molybdenum-vanadium alloyed steel which is characterized by:High wear resistanceHigh compressive strengthVery good through-hardening propertiesVery good toughnessExcellent di.. |
|||
Thermal Conductivity | 26.0 W/m-K @Temperature 400 °C |
180 BTU-in/hr-ft²-°F @Temperature 752 °F |
hardened and tempered condition |
Assab Steels ASP 30 Cold Work Steel ASP 30 is a W-Mo-v-Co alloyed PM high speed steel characterized by:High wear resistanceHigh compressive strength at high hardnessGood through hardening propertiesGood toughnessGood dimensional stabi.. |
|||
Thermal Conductivity | 25.9 W/m-K @Temperature 100 °C |
180 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Schmolz + Bickenbach Cryodur® 2990 Cold Work Die Steel Description: Newly developed ledeburitic cold-work steel with high hardness, good toughness and high tempering resistance combined with high wear resistance.Applications: Cutting and punching tools .. |