Polymer Property : Thermal Conductivity = 184 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 184 W/m-K

@Temperature 20.0 °C
1280 BTU-in/hr-ft²-°F

@Temperature 68.0 °F
Tokuyama Shapal™ SH-15 Sintered Aluminum Nitride