Thermal Properties Metric English Comments
Thermal Conductivity 20.39 W/m-K

@Temperature 20.0 °C
141.5 BTU-in/hr-ft²-°F

@Temperature 68.0 °F
Bohler-Uddeholm BÖHLER K294 MICROCLEAN AISI A11 Powder Metal Tool Steel
Properties: Powder-metallurgical produced cold work tool steel with extremely high wear resistance, good toughness and high compressive strength. The latest generation of powder metal technology ena..