Polymer Property : Thermal Conductivity = 20.92 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 20.92 W/m-K

@Temperature 93.3 °C
145.2 BTU-in/hr-ft²-°F

@Temperature 200 °F
Crucible Steel 446 Chromium Steel
Crucible 446 is a non-hardenable chromium steel which has the highest corrosion and heat resisting properties of the straight chromium steels. This grade is magnetic at all times. Information provi..