Thermal Properties Metric English Comments
Thermal Conductivity 29.1 W/m-K

@Temperature 21.1 °C
202 BTU-in/hr-ft²-°F

@Temperature 70.0 °F
Schmolz + Bickenbach P-20 High Hard Plastic Mold Steel
Description: P-20 High Hard is an improved pre-hardened mold steel that has been specially designed for large plastic molds; Material is forged on a 5000 ton press assuring maximum deformation durin..
Thermal Conductivity 29.1 W/m-K

@Temperature 21.1 °C
202 BTU-in/hr-ft²-°F

@Temperature 70.0 °F
Schmolz + Bickenbach P-20 Modified Plastic Mold Steel
Description: P-20 Modified is an improved pre-hardened mold steel that has been specially designed for large plastic molds; The material is forged on a 5000 ton press assuring maximum deformation du..
Thermal Conductivity 29.1 W/m-K

@Temperature 20.0 °C
202 BTU-in/hr-ft²-°F

@Temperature 68.0 °F
EDRO #3 Prehardened Mold Quality P20 Alloy Steel
EDRO #3™ is a vacuum-degassed, ladle refined, Cr-Ni-Mo- alloyed steel which is supplied in the hardened and tempered condition. EDRO #3™ is manufactured to consistently high quality standards with..
Thermal Conductivity 29.1 W/m-K

@Temperature 20.0 °C
202 BTU-in/hr-ft²-°F

@Temperature 68.0 °F
EDRO #7 Shock Resistant S7 Tool Steel
EDRO #7™ is a chromium-molybdenum steel characterized by: high toughness, good wear resistance, high impact resistance, good through hardening properties, good machinability, and good dimensional s..
Thermal Conductivity 29.1 W/m-K

@Temperature 20.0 °C
202 BTU-in/hr-ft²-°F

@Temperature 68.0 °F
Assab Steels 618 Plastic Mold Material
ASSAB 618 is a vacuum-degassed Cr-Ni-Mo-alloy steel which is supplied in the hardened and tempered condition. ASSAB 618 is manufactured to consistently high quality standards with a controlled sulfu..
Thermal Conductivity 29.1 W/m-K

@Temperature 20.0 °C
202 BTU-in/hr-ft²-°F

@Temperature 68.0 °F
Assab Steels 718HH Plastic Mold Material
IMPAX SUPREME is a premium-quality vacuum-degassed Cr-Ni-Mo-alloyed steel which is supplied in the hardened and tempered condition. IMPAX SUPREME is manufactured to consistently high quality standar..
Thermal Conductivity 29.1 W/m-K

@Temperature 704 °C
202 BTU-in/hr-ft²-°F

@Temperature 1300 °F
Schmolz + Bickenbach Cryodur® 2363 (A-2) Cold Work Die Steel
Description: Cryodur® 2363 is a cold-work steel developed for an excellent combination of wear resistance and toughness and Supplied in the annealed conditionCharacteristics: Good wear resistance; ..
Thermal Conductivity 29.1 W/m-K

@Temperature 21.1 °C
202 BTU-in/hr-ft²-°F

@Temperature 70.0 °F
Schmolz + Bickenbach Holder Block Plastic Mold Steel
Description: Holder Block is a modified AISI-4130 material with higher chromium and molybdenum content specifically designed holder steel for molds and dies and The material is forged on a 5000 ton..