Thermal Properties Metric English Comments
Thermal Conductivity 29.8 W/m-K

@Temperature 200 °C
207 BTU-in/hr-ft²-°F

@Temperature 392 °F
QuesTek® Innovations Ferrium® M54™ Ultrahigh-strength Steel for Structural Applications
Description: Ferrium® M54™ is an ultra high-strength steel for structural applications. Ferrium® M54™ was designed to provide mechanical properties equal to, or better than ultrahigh-strength st..
Thermal Conductivity 29.8 W/m-K

@Temperature 199 °C
207 BTU-in/hr-ft²-°F

@Temperature 390 °F
EDRO #7 Shock Resistant S7 Tool Steel
EDRO #7™ is a chromium-molybdenum steel characterized by: high toughness, good wear resistance, high impact resistance, good through hardening properties, good machinability, and good dimensional s..