Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 22.5 W/m-K @Temperature <=20.0 °C |
156 BTU-in/hr-ft²-°F @Temperature <=68.0 °F |
|
CLAL-MSX ARCAP Anticorrosion AP4 H13 3/4 hard, Drawn Copper Alloy Description: The AP4 grade is less easy to turn than the other grades of ARCAP. It can however be machined without more difficulty than the nickel chromium molybdenum steels.High Corrosion Resistanc.. |
|||
Thermal Conductivity | 22.5 W/m-K @Temperature <=20.0 °C |
156 BTU-in/hr-ft²-°F @Temperature <=68.0 °F |
|
CLAL-MSX ARCAP Anticorrosion AP4 H14 4/4 hard, Drawn Copper Alloy Description: The AP4 grade is less easy to turn than the other grades of ARCAP. It can however be machined without more difficulty than the nickel chromium molybdenum steels.High Corrosion Resistanc.. |
|||
Thermal Conductivity | 22.5 W/m-K @Temperature <=20.0 °C |
156 BTU-in/hr-ft²-°F @Temperature <=68.0 °F |
|
CLAL-MSX ARCAP Anticorrosion AP4 H15 Spring, Drawn Copper Alloy Description: The AP4 grade is less easy to turn than the other grades of ARCAP. It can however be machined without more difficulty than the nickel chromium molybdenum steels.High Corrosion Resistanc.. |
|||
Thermal Conductivity | 22.5 W/m-K @Temperature <=20.0 °C |
156 BTU-in/hr-ft²-°F @Temperature <=68.0 °F |
|
CLAL-MSX ARCAP Anticorrosion AP4 H15 Spring, Rolled Copper Alloy Description: The AP4 grade is less easy to turn than the other grades of ARCAP. It can however be machined without more difficulty than the nickel chromium molybdenum steels.High Corrosion Resistanc.. |
|||
Thermal Conductivity | 22.5 W/m-K @Temperature <=20.0 °C |
156 BTU-in/hr-ft²-°F @Temperature <=68.0 °F |
|
CLAL-MSX ARCAP Anticorrosion AP4 0 Annealed, Drawn Copper Alloy Description: The AP4 grade is less easy to turn than the other grades of ARCAP. It can however be machined without more difficulty than the nickel chromium molybdenum steels.High Corrosion Resistanc.. |
|||
Thermal Conductivity | 22.5 W/m-K @Temperature <=20.0 °C |
156 BTU-in/hr-ft²-°F @Temperature <=68.0 °F |
|
CLAL-MSX ARCAP Anticorrosion AP4 0 Annealed, Rolled Copper Alloy Description: The AP4 grade is less easy to turn than the other grades of ARCAP. It can however be machined without more difficulty than the nickel chromium molybdenum steels.High Corrosion Resistanc.. |
|||
Thermal Conductivity | 22.5 W/m-K @Temperature <=20.0 °C |
156 BTU-in/hr-ft²-°F @Temperature <=68.0 °F |
|
CLAL-MSX ARCAP Anticorrosion AP4 H11 1/4 hard, Drawn Copper Alloy Description: The AP4 grade is less easy to turn than the other grades of ARCAP. It can however be machined without more difficulty than the nickel chromium molybdenum steels.High Corrosion Resistanc.. |
|||
Thermal Conductivity | 22.5 W/m-K @Temperature <=20.0 °C |
156 BTU-in/hr-ft²-°F @Temperature <=68.0 °F |
|
CLAL-MSX ARCAP Anticorrosion AP4 H11 1/4 hard, Rolled Copper Alloy Description: The AP4 grade is less easy to turn than the other grades of ARCAP. It can however be machined without more difficulty than the nickel chromium molybdenum steels.High Corrosion Resistanc.. |
|||
Thermal Conductivity | 22.5 W/m-K @Temperature <=20.0 °C |
156 BTU-in/hr-ft²-°F @Temperature <=68.0 °F |
|
CLAL-MSX ARCAP Anticorrosion AP4 H12 1/2 hard, Drawn Copper Alloy Description: The AP4 grade is less easy to turn than the other grades of ARCAP. It can however be machined without more difficulty than the nickel chromium molybdenum steels.High Corrosion Resistanc.. |
|||
Thermal Conductivity | 22.5 W/m-K @Temperature <=20.0 °C |
156 BTU-in/hr-ft²-°F @Temperature <=68.0 °F |
|
CLAL-MSX ARCAP Anticorrosion AP4 H12 1/2 hard, Rolled Copper Alloy Description: The AP4 grade is less easy to turn than the other grades of ARCAP. It can however be machined without more difficulty than the nickel chromium molybdenum steels.High Corrosion Resistanc.. |
|||
Thermal Conductivity | 22.5 W/m-K @Temperature 93.3 °C |
156 BTU-in/hr-ft²-°F @Temperature 200 °F |
|
Schmolz + Bickenbach Formadur® 2083 Superclean Plastic Mold Steel Description: Formadur 2083 Superclean is an electro slag remelted (ESR) martensitic stainless steel developed for corrosion resistant applications and Supplied in the annealed conditionCharacteristi.. |
|||
Thermal Conductivity | 22.5 W/m-K @Temperature 149 °C |
156 BTU-in/hr-ft²-°F @Temperature 300 °F |
|
Schmolz + Bickenbach CorroPlast® Plastic Mold Steel Description: CorroPlast® is a pre-hardened, free-machining 400 series stainless steel, specifically developed for mold bases for processing plastic; and Supplied in the pre-hardened condition with .. |