Thermal Properties Metric English Comments
Thermal Conductivity 34.8 W/m-K

@Temperature 300 °C
242 BTU-in/hr-ft²-°F

@Temperature 572 °F
Bohler-Uddeholm BÖHLER M268 VMR® Plastic Mold Steel
Description: HBÖHLER M268 VMR is a hardened and tempered plastic mould steel with excellent cleanliness for best polishability. The hardness is constant over the entire cross-section of the steel b..