Polymer Property : Thermal Conductivity = 25.6 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 25.6 W/m-K

@Temperature 204 °C
178 BTU-in/hr-ft²-°F

@Temperature 399 °F
Latrobe LSSâ„¢ H12 Hot Work Tool Steel (ASTM H12)
TLS H12 hot work tool steel is a 5% chromium, general-purpose hot work steel that is characterized by excellent impact toughness. It contains less vanadium than the widely-used H13 hot work tool ste..
Thermal Conductivity 25.6 W/m-K

@Temperature 1000 °C
178 BTU-in/hr-ft²-°F

@Temperature 1830 °F
Haynes 625SQ® Nickel Alloy Sheet
Haynes 625SQ alloy is a solid-solution strengthened superalloy. It is a modification of Haynes 625 alloy designed to enhance resistance to fatigue at temperatures up to approximately 1200°F (649Â..
Thermal Conductivity 25.6 W/m-K

@Temperature 540 °C
178 BTU-in/hr-ft²-°F

@Temperature 1000 °F
Crucible Steel AIRDI® 150 (AISI D2) Tool Steel
Airdi 150 (AISI D2) is an air-hardening, high carbon, high chromium tool steel, heat treatable to HRC 60-62. It offers excellent abrasion resistance, due to a large volume of carbides in the microst..