Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 3.89 W/m-K @Temperature 200 °C |
27.0 BTU-in/hr-ft²-°F @Temperature 392 °F |
|
Assab Steels CALMAX Plastic Mold Material CALMAX is a chromium-molybdenum-vanadium alloyed steel characterized by:High toughnessGood wear resistanceGood through hardening propertiesGood dimensional stability in hardeningGood polishabilityGo.. |