Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 3.60 W/m-K @Temperature 650 °C |
25.0 BTU-in/hr-ft²-°F @Temperature 1200 °F |
|
Gouda Vuurvast AC 85-10 D Dense Refractory Brick Description: A special quality with an extra ordinary resistance to alkali and metallurgical slags, a good resistance to thermal cycling, a good volume stability and high strength at high process te.. |
|||
Thermal Conductivity | 3.60 W/m-K @Temperature 1100 °C |
25.0 BTU-in/hr-ft²-°F @Temperature 2010 °F |
|
Gouda Vuurvast LP 97-3 Dense Refractory Brick Description: A high alumina quality brick containing a limited percentage of chromium oxide for improved slag resistance. The product has a very low silica- and iron oxide percentage so that it can .. |