Thermal Conductivity 0.530 - 0.630 W/m-K

@Temperature 1000 °C
3.68 - 4.37 BTU-in/hr-ft²-°F

@Temperature 1830 °F
Gouda Vuurvast CURON 110 C Dense Refractory Castable
Description: Curon 110 C is a coarse castable. Application: covers for anode baking furnaces.Remarks: These values apply to cast products.Information provided by Gouda Vuurvast.
Thermal Conductivity 0.530 - 0.630 W/m-K

@Temperature 1000 °C
3.68 - 4.37 BTU-in/hr-ft²-°F

@Temperature 1830 °F
Gouda Vuurvast CURON 110 Dense Refractory Castable
Description: Curon 110 is an easily workable castable, especially developed to cast complicated shapes. Because of its low shrinkage, this castable has less tendency to crack.Remarks: These values a..
Thermal Conductivity 0.530 - 0.630 W/m-K

@Temperature 600 °C
3.68 - 4.37 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Gouda Vuurvast CURON 140 GM Dense Refractory Castable
Description: Because of its relatively low Fe2O3 content and its high alumina percentages, this gunning castable can be applied up to 1400°C in slightly reducing atmospheres.Remarks: These values..
Thermal Conductivity 0.530 - 0.730 W/m-K

@Temperature 600 °C
3.68 - 5.07 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Gouda Vuurvast FI 25-15 Insulating Refractory Brick
This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast.
Thermal Conductivity 0.530 - 0.730 W/m-K

@Temperature 600 °C
3.68 - 5.07 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Gouda Vuurvast FI 35-15 Insulating Refractory Brick
This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast.
Thermal Conductivity 0.530 - 0.730 W/m-K

@Temperature 600 °C
3.68 - 5.07 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Gouda Vuurvast FI 45-15 Insulating Refractory Brick
This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast.
Thermal Conductivity 0.530 - 0.630 W/m-K

@Temperature 600 °C
3.68 - 4.37 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Gouda Vuurvast CURON 100 Dense Refractory Castable
Description: Curon 100 is a general purpose castable for temperatures up to 1000°C.Remarks: These values apply to cast products. Also available in gunning variety, marked "GM". Other modification..
Thermal Conductivity 0.530 - 0.630 W/m-K

@Temperature 100 °C
3.68 - 4.37 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast CURON 127 S GM Dense Refractory Castable
Description: Curon 127 S GM gunning castable is characterized by a reasonable strength and a good resistance against slag attack. This castable is applied mainly in boilers and incinerators.Remarks:..
Thermal Conductivity 0.530 - 0.630 W/m-K

@Temperature 100 °C
3.68 - 4.37 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast CURON 145 CC Dense Refractory Castable
Description: This castable is especially developed for strong, large constructions.Remarks: These values apply to cast products.Information provided by Gouda Vuurvast.
Thermal Conductivity 0.530 - 0.630 W/m-K

@Temperature 100 °C
3.68 - 4.37 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast CURON 150 H Dense Refractory Castable
Description: Curon 150 H is composed of a very pure grog combined with a high quality high alumina cement. It is characterized by a good resistance against thermal shock and against reducing operati..
Thermal Conductivity 0.530 - 0.630 W/m-K

@Temperature 1000 °C
3.68 - 4.37 BTU-in/hr-ft²-°F

@Temperature 1830 °F
Gouda Vuurvast CURON 100 C Dense Refractory Castable
Description: Curon 100 C can be applied up to 1000°C, under normal operating conditions and is especially applied in the bottom of electrolytic cells in the aluminum industry.Remarks: These values ..
Thermal Conductivity 0.530 - 0.630 W/m-K

@Temperature 1400 °C
3.68 - 4.37 BTU-in/hr-ft²-°F

@Temperature 2550 °F
Gouda Vuurvast GOLITE 160 GM Refractory Insulating Castable
Description: Golite 180 GM is a gunning mix that can be used up to very high temperatures in reducing conditions.Remarks: These values apply to cast products.Information provided by Gouda Vuurvast.