Thermal Properties Metric English Comments
Thermal Conductivity 30.3 W/m-K

@Temperature 704 °C
210 BTU-in/hr-ft²-°F

@Temperature 1300 °F
Schmolz + Bickenbach Thermodur® 2344 Magnum Hot Work Die Steel
Description: Thermodur® 2344 Magnum is an electro slag remelted (ESR) hot work die steel, designed to meet all die casting industry specificationCharacteristics: Excellent toughness; Excellent re..
Thermal Conductivity 30.3 W/m-K

@Temperature 704 °C
210 BTU-in/hr-ft²-°F

@Temperature 1300 °F
Schmolz + Bickenbach Thermodur® E38K Hot Work Die Steel
Description: Thermodur® E38K is an electro slag remelted (ESR) modified H-11 die steel, developed for hot working applications where maximum mechanical strength (toughness) properties are require..
Thermal Conductivity 30.3 W/m-K

@Temperature 704 °C
210 BTU-in/hr-ft²-°F

@Temperature 1300 °F
Schmolz + Bickenbach Thermodur® 2343 EFS Extra Fine Structure (H-11)- Hot Work Die Steel
Description: Thermodur® 2343 is a single melt Extra Fine Structure (EFS) hot work die steel and Supplied in the annealed conditionCharacteristics: Good toughness; Moderate high-temperature strength..
Thermal Conductivity 30.3 W/m-K

@Temperature 704 °C
210 BTU-in/hr-ft²-°F

@Temperature 1300 °F
Schmolz + Bickenbach Thermodur® 2344 EFS Extra Fine Structure - Hot Work Die Steel
Description: THERMODUR 2344 is a single melt Extra Fine Structure (EFS) hot work die steel; and Supplied in the annealed conditionCharacteristics: Good toughness; Good resistance to thermal shock a..