Thermal Properties Metric English Comments
Thermal Conductivity 31.0 W/m-K

@Temperature 200 °C
215 BTU-in/hr-ft²-°F

@Temperature 392 °F
International Mold Steel DH21 Die Cast & Forging Steel
DH21 is for aluminum die cast dies.Information provided by International Mold Steel
Thermal Conductivity 31.0 W/m-K

@Temperature 20.0 °C
215 BTU-in/hr-ft²-°F

@Temperature 68.0 °F
CoorsTek ADS-995R MidFilm™ 99.5% Alumina Thick Film
Applications: thick films and lasers
Thermal Conductivity 31.0 W/m-K

@Temperature 399 °C
215 BTU-in/hr-ft²-°F

@Temperature 750 °F
EDRO #7 Shock Resistant S7 Tool Steel
EDRO #7™ is a chromium-molybdenum steel characterized by: high toughness, good wear resistance, high impact resistance, good through hardening properties, good machinability, and good dimensional s..
Thermal Conductivity 31.0 W/m-K

@Temperature 399 °C
215 BTU-in/hr-ft²-°F

@Temperature 750 °F
hardened to 57 HRC
Bohler-Uddeholm COMPAX™ AISI S7 MOLD QUALITY Cold Work Steel
Chromium-molybdenum alloyed steelA versatile S7 grade recommended for applications demanding a high degree of toughness and moderate wear resistance. Successfully used for heavy-duty punching and sh..
Thermal Conductivity 31.0 W/m-K

@Temperature 399 °C
215 BTU-in/hr-ft²-°F

@Temperature 750 °F
hardness of 45 HRC
Bohler-Uddeholm UDDEHOLM DIEVAR® Hot Work Tool Steel
Description: Uddeholm Dievar is a high performance chromium-molybdenum-vanadium alloyed hot work tool steel which offers a very good resistance to heat checking, gross cracking, hot wear and plastic..
Thermal Conductivity 31.0 W/m-K

@Temperature 400 °C
215 BTU-in/hr-ft²-°F

@Temperature 752 °F
Assab Steels DIEVAR Hot Work Steel
DIEVAR is a high performance chromium-molybdenum-vanadium alloyed hot work tool steel which offers a very good resistance to heat checking, gross checking, hot wear and plastic deformation. DIEVAR i..
Thermal Conductivity 31.0 W/m-K

@Temperature 20.0 °C
215 BTU-in/hr-ft²-°F

@Temperature 68.0 °F
Assab Steels HOTVAR Hot Work Steel
HOTVAR is a high performance molybdenum-vanadium alloyed hot-work tool steel which is characterized by:High hot wear resistanceVery good high temperature propertiesHigh resistance to thermal fatigue..
Thermal Conductivity 31.0 W/m-K

@Temperature 20.0 °C
215 BTU-in/hr-ft²-°F

@Temperature 68.0 °F
Assab Steels QRO 90 SUPREME Hot Work Steel
QRO 90 SUPREME is a high-performance, chromium-molybdenum-vanadium alloyed hot-work tool steel which is characterized by: Excellent high temperature strength and hot hardnessVery good temper resista..
Thermal Conductivity 31.0 W/m-K

@Temperature 399 °C
215 BTU-in/hr-ft²-°F

@Temperature 750 °F
Schmolz + Bickenbach Cryodur® 2357(S-7) Cold Work Die Steel
Description: Cryodur 2357 is a shock resistant tool steel with excellent toughness and high strength; Suitable for cold and hot work applications up to 1000 °F; and Supplied in the annealed conditi..
Thermal Conductivity 31.0 W/m-K

@Temperature 300 °C
215 BTU-in/hr-ft²-°F

@Temperature 572 °F
Quenched and Tempered
Schmolz + Bickenbach Cryodur® 2767 Cold Work Die Steel
Description: High hardenability and toughness, highly suitable for polishing, texturing and EDM machining. We recommend the use of Cryodur® 2767 (ERS) for extreme demandsApplications: Cutlery dies,..