Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 35.1 W/m-K @Temperature 100 °C |
244 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Bohler-Uddeholm BÖHLER M268 VMR® Plastic Mold Steel Description: HBÖHLER M268 VMR is a hardened and tempered plastic mould steel with excellent cleanliness for best polishability. The hardness is constant over the entire cross-section of the steel b.. |