Thermal Conductivity 37.2 W/m-K

@Temperature 204 °C
258 BTU-in/hr-ft²-°F

@Temperature 400 °F
Schmolz + Bickenbach Thermodur® 2714 Extra Fine Structure - Hot Work Die Steel
Description: Thermodur 2714 is an Extra Fine Structure (EFS) nickel based tool steel.Characteristics: Excellent high temperature strength; Good toughness; and Good resistance to thermal shockApplica..