Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.590 W/m-K @Temperature 650 °C |
4.09 BTU-in/hr-ft²-°F @Temperature 1200 °F |
|
Pyrotek Dry Cathode Barrier Material In the presence of cryolite, Dri-Barrier Mix is designed to form a viscous layer on its surface which prevents further penetration. The freezing isotherm sustained in Dri-Barrier Mix decreases the .. |
|||
Thermal Conductivity | 0.590 W/m-K @Temperature 400 °C |
4.09 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Pyrotek Pyrocast AR Castable Refractory Pyrocast AR is a fused silica castable refractory inert to liquid aluminum and its alloys. It is a high strength material offering resistance to erosion and mechanical damage. Parts cast from Pyro.. |
|||
Thermal Conductivity | 0.590 W/m-K @Temperature 400 °C |
4.09 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Pyrotek Pyrocast AR FINE Castable Refractory Pyrocast AR Fine is a fine-grain fused silica castable, offering similar insulation properties, yet lighter weight that the Pyrocast AR formulation. Pyrocast AR Fine is suited for thin wall casting.. |
|||
Thermal Conductivity | 0.590 - 0.690 W/m-K @Temperature 100 °C |
4.09 - 4.79 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast CURON 160 HS GM Dense Refractory Castable Description: This gunning castable has a high volume stability up to high temperatures. In addition Curon 160 HS GM has an excellent thermal shock resistance and abrasion resistance (9-12 cm3 accord.. |
|||
Thermal Conductivity | 0.590 W/m-K @Temperature 538 °C |
4.09 BTU-in/hr-ft²-°F @Temperature 1000 °F |
ASTM C182 |
BNZ Materials BNZ-32 Insulating Firebrick BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |