Thermal Conductivity 41.33 W/m-K

@Temperature 93.3 °C
286.8 BTU-in/hr-ft²-°F

@Temperature 200 °F
International Mold Steel NAK55 Precipitation Hardened Mold Steel
Description: NAK55 is a precipitation, or age-hardened mold steel with a through hardness of approximately 40 HRc. NAK55 is ideal for use in plastic and rubber molds and other applications where imp..
Thermal Conductivity 41.33 W/m-K

@Temperature 93.3 °C
286.8 BTU-in/hr-ft²-°F

@Temperature 200 °F
International Mold Steel NAK80 Precipitation Hardened Mold Steel
Description: NAK80 is a precipitation or age-hardened mold steel with a uniform through hardness of approximately 40 HRc. It is super clean, Vacuum-Arc Remelted steel with uniform grain structure, u..